LIGA ZINKSTEARAT 101
A non-reactive hydrophobic agent produced by precipitation with a high specific surface and excellent long-term effectiveness, primarily for limestone cement plaster. The dosage is 0.1% to 1%. In order to ensure optimal effectiveness, sufficient time is necessary for mixing the dry mortar. Zinc stearates in plaster are light algicides.
LIGA ZINKSTEARAT 501
A type of zinc stearate with considerably improved flowing properties. In comparison to LIGA ZINKSTEARAT 101, the dry mortar can be mixed more easily. The dosage is slightly higher.
LIGAPHOB CSG
Another non-reactive stearate type produced by precipitation with a high specific surface for mineral plasters. At 0.2 to 1% the dosage is higher than of LIGA ZINKSTEARAT 101. However, there are advantages in the preparation of dry mortar.
LIGA MAGNESIUMSTEARAT TECHN.
Standard grade with very good water repellent properties. Suitable for application in most cement bonded building materials. Very good free-flowing and dosing properties.
LIGAPHOB MSG
Finely powdered, precipitated grade of Magnesium stearate. Application as substitute for precipitated Zinc stearates. Very efficient hydrophobic agent with significantly less dosage compared to LIGA MAGNESIUMSTEARAT TECHN.
LIGASTAR AL D2
LIGASTAR AL DT
A slightly reactive hydrophobic agent primarily for insulating and repair plasters. Aluminium stearates can be mixed well in dry mortar. The dosage is between 0.1 and 1%.